Oak dged board:

1)Oak dged board:

Size: length -from 2500 mm – 3000 mm (step 100 mm);

2300 mm – 2450 mm (step 50 mm);

2000 mm – 2250 mm (step 50 mm);

width: 140 mm; 150 mm; 160 mm … and more (step 10 mm); thickness: 25 mm.

Humidity: fresh cut

Packing: on pallets, constricted by strips.

Grade: I, II — face clean, without knots and sapwood.

On the second side (not the front) are allowed: a living a knot to 10mm, not facing the front of the no closer than 10 mm from the edge of the edge or end, cracks at the ends — up to 3 cm on one side of the board, but not more than 10% of the consignment, sapwood not on the front side up to 1/3 of thickness.

Not allowed: wavy cut, sapwood, knots and side rotten, dark knots, pith, crust, wormholes, mold, rot, yellow fungus, cracks, whiteness, mechanical damage and other defects. Volume: from 35 m3 per month

2)Oak edged board:

Size : from 2500 mm – 3000 mm (шаг 100 mm);

2300 mm – 2450 mm (шаг 50 mm)2000 mm – 2250 mm (шаг 50 mm);

width: 140 mm; 150 mm м; 160 mm … and more (шаг 10 mm); thickness: 25 mm.

Humidity: 10% (+/- 2%)

Packing: on pallets, constricted by strips.

Grade: I, II — face clean, without knots and sapwood. On the second side (not the front) are allowed: a living a knot to 10mm, not facing the front of the no closer than 10 mm from the edge of the edge or end, cracks at the ends — up to 3 cm on one side of the board, but not more than 10% of the consignment, sapwood not on the front side up to 1/3 of thickness.

Not allowed: wavy cut, sapwood, knots and side rotten, dark knots, pith, crust, wormholes, mold, rot, yellow fungus, cracks, whiteness, mechanical damage and other defects.

3)Oak edged planks (strips):

Sizes (length/width/thickness): 320;370;420mm x 53mm x 27mm 320;370;420mm x 63mm x 27mm 370;420;470mm x 73mm x 27mm

420;470;520mm x 83mm x 27mm

Humidity: 10% (+/- 2%)

Packing: on pallets, constricted by strips.

Grade: one side clean. On the second side, not the front, allowed: knots live, black knots up to 10mm no closer than 8 mm from the edge of the edge or end, sapwood not on the front side up to 1/3 of thickness. Not allowed: wavy cut, sapwood, knots and side rotten, dark knots, pith, crust, wormholes, mold, rot, yellow fungus, cracks, whiteness, mechanical damage and other defects.

Volume: from 35 m3 per month